In the metallurgy of iron, the charge of roasted ore, coke and limestone is taken in which ratio in the blast furnace?
A8 : 4 : 1
B4 : 8 : 1
C1 : 4 : 8
D2 : 1 : 1
Answer & Solution
Correct answer: A. 8 : 4 : 1
1. In the blast furnace the charge is fed through the hopper at the top.
2. It consists of roasted ore, coke and limestone.
3. These are taken in the ratio 8 : 4 : 1 respectively.
_Source: Samacheer Kalvi (TN SCERT) Class 10 Science, Unit 8 Periodic Classification of Elements "Metallurgy of Iron", p.124_
Related questions
In cathodic protection against corrosion, the metal that is deliberately attached to corroWhy does dilute or concentrated nitric acid fail to react vigorously with aluminium metal?During the smelting of iron in the blast furnace, what is the main role of the limestone (Using electronegativity values F = 4.0 and Na = 0.9 (approx 1.0), the Na-F bond is best deIn Mendeleev's atomic-mass arrangement, argon (39.95 amu) was placed before potassium (39.Which of these alloys is a non-ferrous copper alloy made of copper and zinc?In the modern periodic table, the sixth period (atomic numbers 55 to 86) contains how manyA substance added to an ore to lower the fusion temperature and combine with the gangue is