In the Mortar Bar Expansion Test (Stanton) cited in §2.2.12, the aggregate is considered HARMFUL if the specimen expansion exceeds:
A{'text': '0.005 percent after 3 months', 'label': 'A'}
B{'text': '0.0005 percent after 3 months', 'label': 'B'}
C{'text': '0.05 percent after 6 months', 'label': 'C'}
D{'text': '0.5 percent after 12 months', 'label': 'D'}
Answer & Solution
Correct answer: A. {'text': '0.005 percent after 3 months', 'label': 'A'}
1. §2.2.12(b) Mortar Bar Expansion Test: 'The aggregate under test is considered harmful if the expansion is more than 0.005 percent after 3 months or more than 0.1 percent after six months.'
2. The specimen is a 25 mm × 25 mm bar measured at 1, 2, 3, 6, 9 and 12 months.
_Source: IGNOU ET-522 Block-1 Unit-2 Aggregates, §2.2.12(b), p. 25_
Related questions
Per the source, three thermal properties of aggregates are named; the one most important fPer §2.3.2(iii), in the Aggregate Impact Value test the standard hammer falls from a heighPer §2.3.2(i), in the Aggregate Crushing Value (ACV) test the aggregate sample is loaded uPer §2.3.1(v) of the source, the specific gravity of an aggregate sample is computed by:Per §2.2.14, the Fineness Modulus range that corresponds to MEDIUM sand is:Per Abrams (cited in §2.2.14), the Fineness Modulus of an aggregate is obtained by:Per the prevention measures in §2.2.12, the alkali content of cement to limit alkali-aggrePer §2.2.12, the chief reactive component in aggregates that drives the alkali-aggregate r